Snap-shots of YBCO Preparation and
Characterization
1.World Wide Web and library search for background information
2. Weight of starting compounds is determined
3. Powder components are mixed and carefully ground
4. Mixed powder is heated in furnace for 24 hrs. Powder is reground and the
procedue is repeated 2-3 times until materials has a uniform gray color.
4. X-ray Diffraction and Raman Scattering (above, Thanks to Prof. J. J. Federici's
Lab.) are used to characterize sample.
5. The Meissner Effect is a key test of superconductivity and serves as a neat demonstration